{"id":5949,"date":"2024-05-17T14:03:40","date_gmt":"2024-05-17T06:03:40","guid":{"rendered":"https:\/\/www.textile-fabric.com\/archives\/5949"},"modified":"2024-05-17T14:03:40","modified_gmt":"2024-05-17T06:03:40","slug":"precautions-for-maintenance-and-operation-of-preshrinking-machine","status":"publish","type":"post","link":"https:\/\/www.textile-fabric.com\/?p=5949","title":{"rendered":"Precautions for maintenance and operation of preshrinking machine"},"content":{"rendered":"<p>Precautions for maintenance and operation of preshrinking machine<\/h1>\n<p>                     11 Maintenance <BR> (1) The humidity of the fabric in the humidification box is uneven. Check: <BR> \u2460 Whether the spray and steam pipes are blocked.  <BR> \u2461 Whether the steam pressure and water pressure are high and low suddenly.  <BR> \u2462 Whether the main and passive guide rollers in the wet box are bent or damaged, whether the journals and bearings are damaged or the oil is cut off.  <BR> (2) If a single pre-drying cylinder produces wrinkles and abnormal sounds, you should check: <BR> \u2460 Whether the water bucket or siphon in the drying cylinder is damaged.  <BR> \u2461 Whether the drying cylinder is deformed.  <BR> \u2462Whether the journal and bearing of the dryer cylinder are worn or the oil is cut off.  <BR> (3) If the blanket is deflected or wrinkled, check: <BR> \u2460 Whether the blanket tension roller is horizontal or bent, and whether it is perpendicular to the center line.  <BR> \u2461 Whether the felt tension roller, felt drying cylinder journal, and bearings are worn or oil-cut.  <BR> \u2462Whether the felt drying cylinder is conical or oval.  <BR> \u2463Whether the blanket is partially worn or uneven in thickness.  <BR> (4) If the rubber blanket is deviating, check: <BR> \u2460 Whether the levelness of the pressure roller is within the standard range.  <BR> \u2461 Whether the perimeter of both sides of the rubber blanket is consistent.  <BR> \u2462 Whether the wear and aging on both sides of the rubber blanket are consistent, and whether there are ruffles.  <BR> If there is no above problem, you should adjust the rubber blanket, adjust the tension at both ends of the roller, loosen the end that deviates outward, or adjust the pressure on both sides of the cloth feed roller <BR> and pressurize the end that deviates outward.  <BR> (5) The shrinkage of the finished fabric after preshrinking is uneven. You should check: <BR> \u2460 Whether the steam pressure is high and low, and whether the moisture supply is uniform.  <BR> \u2461 Whether the temperature of the pre-shrinking machine is uniform.  <BR> \u2462Whether the speed difference of the feed roller and retard roller is stable.  <BR> \u2463Is the pressure stable?  <BR> \u2464Whether the hydraulic roller, cloth feed roller, retard roller, etc. are bent or elliptical, and whether the bearings are damaged or have oil outage.  <BR> (6) If the fabric shrinkage after pre-shrinking and finishing is unqualified, you should check: <BR> \u2460 Whether the moisture supply rate of the fabric meets the requirements.  <BR> \u2461Whether the pressure meets the requirements.  <BR> \u2462Whether the overfeeding amount is appropriate.  <BR> (7) All kinds of bearings of the pre-shrinking machine should be lubricated once a week and inspected once a year.  <BR>\u300021 Operation Precautions<BR>\u3000(1) Corresponding preparations and inspections should be made before driving.  <BR> (2) Open the machine first, adjust the corresponding pressure and temperature required for pre-shrinking, and then introduce the fabric for pre-shrinking and finishing.  <BR> (3) Check the fabric preshrinkage regularly.  <BR> (4) After the fabric is pre-shrunk and finished, the machine should still be run empty, relax the pressure, turn off the steam, and lower the temperature of each roller before stopping.<br \/>\n                     AAAKY, 7II56U65 <\/p>\n<p>Extendedreading:<a href=\"https:\/\/www.brandfabric.net\/full-dull-nylon-dobby-2-5-layer-with-silver-coated-fabric\/\">https:\/\/www.brandfabric.net\/full-dull-nylon-dobby-2-5-layer-with-silver-coated-fabric\/<\/a><br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedreading:<br \/>Extendedread<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Precautions for maintenance and operation of preshrinking machine 11 Maintenance (1) The humidity of the fabric in the humidification box is uneven. Check: \u2460 Whether the spray and &hellip;<\/p>\n","protected":false},"author":1,"featured_media":0,"comment_status":"","ping_status":"","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[5],"tags":[46],"class_list":["post-5949","post","type-post","status-publish","format-standard","hentry","category-textile-fabric-news","tag-db"],"_links":{"self":[{"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=\/wp\/v2\/posts\/5949","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=5949"}],"version-history":[{"count":0,"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=\/wp\/v2\/posts\/5949\/revisions"}],"wp:attachment":[{"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=5949"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=5949"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.textile-fabric.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=5949"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}